Guenter According to Johann Lau's book on conductive adhesives, they are mainly epoxy resins, although other resins may also be used. If you are very interested in this subject, the book is fantastically good and covers all aspects of conductive adhesives. Best regards Brian Guenter Grossmann wrote: > > Hi all > > What polymers are used for anisotropic adhesives? > > Best regards > > Guenter > > Guenter Grossmann > Swiss Federal Institute for Materials Testing and Research EMPA > Centre for Reliability > 8600 Duebendorf > Switzerland > > Phone: xx41 1 823 4279 > Fax : xx41 1823 4054 > mail: [log in to unmask] > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## -- Brian Ellis Protonique SA PO Box 78 CH-1032 Romanel-sur-Lausanne, Switzerland Voice: +41 21-648 23 34 Fax: +41 21-648 24 11 E-mail: [log in to unmask] URL: Technical and consultancy divisions: http://www.protonique.com Web services division: http://www.protonique.com/webserv ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################