You hit the nail on the head with the phrase "machine grounded properly". That is the key. Proper grounding will eliminate the problem. EOS/ESD-S6.1-1991 is a good Grounding Recommended Practice. Contact your equipment manufacturer for ESD grounding information. Al Cash -----Original Message----- From: Stephen R. Gregory [mailto:[log in to unmask]] Sent: Friday, March 03, 2000 7:04 PM To: [log in to unmask] Subject: Re: [TN] Spec for "Lumps" on PCB In a message dated 03/03/2000 6:40:05 PM Central Standard Time, [log in to unmask] writes: > This is where polyimide stencils with appropriate blades come to very much > their own . > (unless yo' dispense, hehehe) > Funny how things go around .... > and those base carbon brushes under exit , please . > That' reminds me ' ll flush a contact on net , don't shoot ! > > paul Hi ya' buddy! I'm still amazed at your dispensing processes! I know without a doubt that you have them down (article in Advanced Packaging a while back about your place)...I often wonder why we (in the US) have never gone that route? I suppose "necessity is the mother of invention" has a big part in it. As you once pointed out, being "down-under" you don't have the luxury of having a bunch of stencil vendors at your whim... Still, not having one of them polyimide stencils on hand to see things for myself, I wonder if it really is as big a problem as what's being portrayed? I understand that the stencil handles metal squeegees, and if you have your machine grounded properly, what's the deal? Maybe someone from K.J. Marketing (if they've ears here) can address this? -Steve Gregory- ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################