Does the component contact the board? Requirements for adhesive bonding change if the component is elevated. The IPC-A-610 requirement for class three is 50% of the length of the component and 25% of the diameter. Adhesion (before and after testing) must be evident. Elevated components weighing more than 7g must be bonded in at least four places evenly spaced around the component and at least 20% of the total periphery must be bonded, adhering to both the board and the component. -----Original Message----- From: phil bavaro [mailto:[log in to unmask]] Sent: Monday, March 20, 2000 5:05 PM Subject: Electrolytic Capacitor Staking Requirements OK, I know, I know. Why is anyone still using thru hole parts which have to be bonded to the board......!! Well. all I can say is that we are and the question I have for this group is what are the requirements for how much and how high. Here's the background info: An automotive electronics circuit card has about seven very tall electrolytic caps on it which need to be secured to the board so that the vibration does not sever the two leads on these parts. Historically I have always asked that these be bonded 360 degrees around the perimeter and a minimum of 50%, up to a maximum of 100% of the height of the part using a thixotropic UV cure adhesive. This way the part could not bend or move at all. Using this criteria, I have never seen a failure as a result of the bonding. Here's the problem: A new engineer decides to minimize the adhesive amount (due to cycle time of course) so that just it connects the board and the bottom of the part only (maybe as high as .15" total which only allows about .10" of contact to the body of the part. These parts are .75" tall. The new engineer feels justified because the products which were bonded this way made it thru a HALT test exposure without electrical failures. I look at the assemblies which are supposedly OK and find that the adhesive has broken loose from the pwb on at least five out of the seven parts and what is remaining on the parts have fracture lines as well. I consider this condition unacceptable and feel that after environmental testing, adhesive bonding should remain intact 100%. Am I right or should I yield since the assemblies made it thru the HALT testing? What bonding requirements do you impose for these type of parts All comments are welcome. ----------------------------------------------------- Click here for Free Video!! http://www.gohip.com/freevideo/ ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################