Jason I agree with Ed. We have used this process for many years with very little problems on soldering ceramic substrate into RF housings. The only issues that I know of and we have had them many times is the availablity of the liquids and the expense of them. You might be better off with forced convection if you have any concerns with costs. -----Original Message----- From: Edward J. Valentine [mailto:[log in to unmask]] Sent: Wednesday, March 01, 2000 3:34 PM To: [log in to unmask] Subject: Re: [TN] vapor phase reflow Jason - With all due respect to Mr. McMonagle, vapor phase reflow with preheating (an integral part of many units since the mid-80's), can produce excellent results in very dense assemblies and backplanes. The chief advantage is its very even heat distribution over the assemble. The highest temperature fluorinated liquid that I am familiar with is FC-71, which has a higher boiling temperature than the 215C (419F), FC-70. The FC-71 is 250C (495F). The liquids are very expensive, but the only fluids that were/are regulated were the secondary fluids (Freons), not the Primary fluorinated fluids since they are not a HFC or cause any effect on the ozone, nor are they a regulated contaminant,but that may vary at some locales. Generally, forced convection is the preferred reflow process, but it is not a panacea for all applications. If you would like to discuss some more, please feel free to contact me offline. Ed Valentine Electronics Manufacturing Solutions 8612 Mourning Dove Road, Raleigh, NC 27615 Phone: (919) 270-5145, Fax: (919) 847-9971 Email: [log in to unmask] Website: http://www.ems-consulting.com ----- Original Message ----- From: Jason Gregory <[log in to unmask]> To: <[log in to unmask]> Sent: Wednesday, March 01, 2000 8:53 AM Subject: [TN] vapor phase reflow > Hello techies! > > I am looking for anyone who has performed any qualifications on the advantages/disadvantages of vapor phase reflow. Particularly dealing with higher temp alloys. Is it the way to go? Is convection better? Who are the major manufacturers? Are silicon castments to keep the bottomside components from falling off mandatory? Any replies are GREATLY appreciated. > > Jason Gregory > Production Manager > Electrospec > (713)784-4900 > (713)784-1194 fax > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################