TOE, Did you have success with your cover sheet removal query? DB. TOE /Torben Østeraa wrote: > Dear Technetters, > > I would like to know about experiences, good or bad, > with equipment for removal of photoresist cover sheet. > > Performance and reliability with thin core, > e.g. 2mil 1oz/1oz 'kapton', is of special interest. > > thank you for your help, > > regards > > Torben Østeraa > Printca AS > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## -- Dave Brown Quality Manager RexCan Circuits [log in to unmask] 1-613-969-0009 161 Bridge St. E. Belleville Ont. K8N 5B6 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################