Rick, A few years ago the IPC Blue Ribbon II committee addressed this subject. Tests performed by NSA was included in the final report. Contact David Bergan at IPC for the report and the NSA data. Bottom line no measled PWB's failed during the NSA tests. Arny Andrade Sandia Labs, retired ----- Original Message ----- From: Howieson, Rick <[log in to unmask]> To: <[log in to unmask]> Sent: Tuesday, February 01, 2000 1:45 PM Subject: [TN] Measling > IPC states measling is not cause for rejection. Anyone out there know > where I can get supporting data that documents testing performed to come > to this conclusion? All help is appreciated. > > Rick Howieson > http://www.gt-corp.com > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################