TechNet, We have some SMT CCAs which we receive with Entek OSP coating. The vias on the PWB are not solder masked nor during assembly processing are they screened and pasted. After convection oven reflow, is there still some Entek on the vias or is the OSP removed by the processing? The CCAs are later conformally coated which puts down 1-5 mils of type AR protection on the vias. However the vias underneath large QFPs do not get conformally coated by the Nordson sprayer. Is there a reliability concern here? Also, after 120 hours of humidity/temp cycling, the tin-lead pasted areas exhibit some white residue while the non-solder masked and non-conformally coated Entek areas appear fine. In anyone's experience, is there a long term issue for Class 3 goods? Stu Korringa Smiths Industries Grand Rapids, Mi [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################