See comments below. (Embedded image moved Eric Kalgren <[log in to unmask]> to file: 01/28/2000 02:44 PM pic16377.pcx) To: [log in to unmask] cc: (bcc: Kenneth Kirby/ElectrovertUS/Cookson) Subject: [TN] Grainy Looking Wave Solder Joint Once again I supplicate myself before the altar of TechNet..... We are seeing dull/grainy looking solder joints coming off the wave solder machine (Electrovert EconoPak+). These are high-rel, high mix PCAs that are required to conform to the old NHB5300. Specifically the bit about having "bright and shiny" solder joints. I am currently profiling the PCA to have an avg topside temp of 250 deg F when it hits the start of the solder wave. I suspect, based on my readings of Klein-Wassink that the joints are cooling too slowly (some of these PCAs have huge ground planes covering the entire top and bottom side). That and the fact that the majority of the dull-looking joints are on heavy components? My questions: 1) Should I be profiling to a lower temp? Yes, if you can still get good topside fillets. Also keep the conveyor speed up to minimize the dwell time but still get top side fillets. 2) Does anyone have any pet methods for helping to cool the joints more quickly? A set of cooling fans after the solder pot is all that is needed. Electrovert offers cooling fans that mount just outside the end cap but you may need to add a set between those and the solder pot also. I have been to your your shop before and know Bob Crain. Give me a call if you need more info. Ken Kirby Speedline Technologies We are working on getting the spec relaxed, but I think that I should be able to hit any spec with the correct profile. Humbly, Eric Kalgren BFGoodrich Aerospace Data Systems Division [log in to unmask] (505) 938-5139 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################