Agree ; works fast (validation desirable), "rinse" needed ; "inventive" clients you have Doug : excellent job security . paul -----Original Message----- From: Douglas Pauls [mailto:[log in to unmask]] Sent: Friday, 25 February 2000 0:29 To: [log in to unmask] Subject: Re: [TN] Cleaning of edge board connectors In a message dated 02/23/2000 4:28:52 PM US Eastern Standard Time, [log in to unmask] writes: > but your local jeweler/supply does sell silver and gold cleaning compounds > and aids . > Yes, they do. But be very cautious. Most are too aggressive or have surfactant compounds that are detrimental if not completely removed. I had a client once who asked if they could use Tarn-X as a flux. I shudder even thinking about it. Doug Pauls ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################