Hi Todd! Your interpretation is correct in that JSTD-001 requires (the "must" word is used) that the solderability of the components be ensured. That can be done in one of three ways: 1) the component supplier gives you confirmation that the components will meet the requirements of JSTD-002A ; 2) you conduct testing that the components will meet the requirements of JSTD-002A; 3) you skip solderability testing and pretin the components prior to their use in the assembly operation. If a component vendor has a great plating process and will provide you documentation that the components will meet JSTD-002A despite their being X Xyears in storage then that meets the requirements or if you don't want to conduct any solderability testing and choose to pretin then that also meets the requirements (if the components have solderability problems they will show up during pretinning!). You should select the method of ensuring solderability which best fits your schedule, cost, and assembly process. The easiest and most cost effective method is teaming with your component vendor. Hope this helps. Dave Hillman ANSIJ-STD-002A Committee CoChair [log in to unmask] Todd Wakeland <[log in to unmask]> on 02/09/2000 06:23:03 PM Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to Todd Wakeland <[log in to unmask]> To: [log in to unmask] cc: Subject: [TN] Solderability Requirements To all, For purchased components we impose solderability requirements of J-STD-002 on our suppliers. Most of the time we use these purchased parts in a timely manner and do not experience solderability problems. More recently, however, we are having to make decisions about whether or not we can use components from stock that are 1-2 years old. There seems to be some confusion within my group as to whether or not "solderability testing" needs to be performed to determine whether these parts are still solderable. In reading J-STD-001B para 5.2 Solderability, the last sentence says "When a pre-tinning and inspection operation is performed as part of the documented assembly process, that operation may be used in lieu of solderability testing." Based upon this statement, would it be acceptable to tin and inspect a sample of each aged lot based upon an established sampling plan (that we would create) Vs having to go through the riggers of solderability testing per J-STD-002. Based upon what I have read it appears that we will in fact need to validate the solderability of these parts based upon their age? Any clarification would be welcome. Todd Wakeland TRW ASD [log in to unmask] ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################