Hi Lou and All, <de-cloaking> We're using a Leica refractometer to measure Kyzen's Aquanox XJN concentration in our in-line cleaner. Automatic controllers are great and if you run enough product (or chemistry) they can sure pay for themselves in a hurry. The biggest hurdles I've had to overcome with using the refractometer had more to do with training the operators than the chemistry. My question, why the change? Are boards or assemblies failing after cleaning or is this part of a general process review? As Alain pointed out, there are several methods of achieving the same result (to varying degrees) - knowing when to dump the sump or knowing how much to add. It depends on your specific needs - greater precision & control vs. cost (several models) vs. ease/speed of use. It's like Rudy said, the titration may come out as a false positive (bath okay) but if the boards aren't clean it doesn't really help. Hans ~~~~~~~~ Hans M. Hinners Materials (& Process!) Engineer Warner Robins - Air Logistics Center/Avionics Production Division Manufacturing Branch (LYPME) 380 Second Street, Suite 104 (Building 640) Robins AFB, GA 31098-1638 912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7164 (Fax) mailto:[log in to unmask] > -----Original Message----- > From: Lou Hart [SMTP:[log in to unmask]] > Sent: Monday, February 07, 2000 11:39 > To: [log in to unmask] > Subject: [TN] Saponifier concentration measurement > > Technetters, how do you measure saponifier concentration in a board > assembly cleaning machine? We've been using a refractometer to measure > degrees Brix, but this is appears to be a "legacy" method. I've been > hearing titration would be the way to do it. Please comment. Lou Hart QA > manager, Compunetix 412-858-6184 > ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################