Hello technet, Hopefully there are some bored Sunday e-mail surfers out there. We have an issue with acceptability standards on coiled transformers and the issue is this: all of our red-coated x-formers have areas where the protective coating is nicked or the heat from the iron during rework is peeling the coating back and exposing copper. Is there an IPC standard dictating acceptability? Please help!! Jason Gregory Production Manager Electrospec 8626 Westpark Houston, TX. 77063 ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################