Bob: I have encountered the same problem that you have indicated. For a NASA application I have used specification A-A-55485/6A mounting pads. I have used A-55485/06-010D under CK06 parts and A-55485/06-048D under CK05 parts. This spec is a replacement for the old Mil-M-38527/60 spec. The spacers are made of diallyl phthalate and can be purchased from a number of sources as listed in the spec. The spacers remain permanently under the parts. The spacer holds the part off the board while allowing a topside fillet to form while wavesoldering. The need for this spacer has diminished as both the CK05 and CK06 parts can be purchased with an integral standoff. However, the high rel parts M123A01 and M123A02 are not available with the standoff and therefore the spacer is necessary. Respond if you need more help. Bill Kasprzak Moog Inc. > -----Original Message----- > From: Bob Crain [SMTP:[log in to unmask]] > Sent: Thursday, February 03, 2000 5:17 PM > To: [log in to unmask] > Subject: [TN] Temporary stand offs for wave solder > > We are converting some old hand solder aerospace PCA designs to wave > solder. The transistors and CKR05 type capacitors need temporary stand > offs. > > We cannot use standard dissolvable spacers because we use alcohol solvent > cleaning and are not allowed to use water. > > Suggestions? One thing I would like to consider is a high temperature, > non-silicone, non-sulfur rubber sheet in thicknesses of .030" and .050." > Any ideas for the best material to use? Are there any removable clips that > fit over the parts to hold them up? > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for > additional > information. > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or > 847-509-9700 ext.5365 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or 847-509-9700 ext.5365 ##############################################################