I have used the Getek and the Rogers 4003 (4350) series materials. Both have excellent properties depending on the affects you are most concerned about. The 4003 materials have a performance edge (better Er and loss tangent), but the Getek was more cost competitive for use when I last checked in to these material. I have never used the Nelco equivalent or the Tetra 2 materials. Use a material that the fabricator you plan to work with is familiar with to minimize fabrication problems and cost. Jeffrey A. McGlaughlin Sr. PCB Designer Battelle Memorial Institute Columbus Ohio [log in to unmask] -----Original Message----- From: Alexis Meehan [SMTP:[log in to unmask]] Sent: Thursday, 03 February, 2000 12:21 To: [log in to unmask] Subject: [DC] High-Speed Materials We are currently researching materials that will handle high-speed circuits (over 1 ghz) better than the current FR4 that we've been using. We've talked to our fab vendors and they are recommending alternatives such as Getek, Tetra 2, and Rogers 4350. Now I'd like to hear from the end users. Has anyone out there gone through a similar transition? What were your experiences with the more costly materials? Any input would be greatly appreciated. ******************** Alexis Meehan PCB CAD Mgr. 408-328-4595 [log in to unmask] LuxN, Inc. 570 Maude Court Sunnyvale, CA 94086