In a message dated 12/02/1999 2:54:44 PM US Eastern Standard Time,
[log in to unmask] writes:
>
> It seems to be my week for strange requests.
> Does anyone know of a fungicidally treated FR4 laminate? Or of any
> fungicidal treatment which can be applied to an assembled circuit board.
>
I can't really see the need for a fungicide. Most IPC specs have the
requirement that the base material, such as laminate, mask, and coating be
non-nutrient in nature, which means it would not support growth of a fungus.
Doug Pauls