You can try the following witches brew - it works but must be made fresh
every few days also the HF must be handled with care.


100 mls Ardrox 204 ( or any methylene chloride gel based paint stripper)

11 g Phenol
2 mls of 60% Hydrofluoric acid

regards
Chris Evans