Here in the aerospace business, we ALWAYS bond or otherwise secure tantalum
capacitors for the reason you mention - vibration.
R. G. Blomberg
Honeywell -SASSO
Staff Production Engineer
(727) 539-5534 voice
727-539-4469 Fax
[log in to unmask]
-----Original Message-----
From: Jean-Francois Bissonnette [mailto:[log in to unmask]]
Sent: Thursday, December 09, 1999 8:04 AM
To: [log in to unmask]
Subject: [TN] Tantalum capacitors
Hi Techneters!
Maybe the next question as an obvious answer but I need to know
(You see they just gave me QC inspector job here with nothing else
than an IPC-A-610 Class "A" instructor course to go with. No other
means of training, well someone helps but it's not is job.
That's why my questions may sometimes seem a little basic... sorry!).
Do the big tantalum capacitors need to be secured on the boards? I suppose
yes but some people who claim having years of experience say that
no (Hum!). Wont the vibrations give a hard time to that kind of capacitors?
BTW, anyone know a gook way to get information on QC.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|