Some double sided kits I have built for ham radio applications used the
component leads for feed throughs, you just provide a good solder fillet to
the pads on both sides of the board. In other cases a small wire was used,
but a rivet might have been easier since it would be cut to size, it should
also be pre-tinned.
Bill Dieffenbacher
> ----------
> From: Alain Savard[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Alain Savard
> Sent: Tuesday, December 07, 1999 9:06 AM
> To: [log in to unmask]
> Subject: Re: [TN] vias and plated through holes for homemade board.
>
> How about trying copper rivets and the solder to the trace/land?
>
> Just a tought,
>
> Alain Savard, B.Sc.
> Chemical Process Analyst
> CAE Electronics Ltd.
> e-mail: [log in to unmask]
>
>
> -----Original Message-----
> From: Jean-Francois Bissonnette [mailto:[log in to unmask]]
> Sent: December 6, 1999 5:05 PM
> To: [log in to unmask]
> Subject: [TN] vias and plated through holes for homemade board.
>
>
> Hi Techneters!
>
> From time to time I like to desing some little boards, just for the fun of
> it.
> I've been looking for a way to get plated through holes for double sided
> boards.
> Is there anything that exists and available in big quantity that I can
> use?
>
> Thank You!
>
> JF
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|