You can remove the tin/lead with a strong caustic. Check Circuit Technology
Corp's website at http://www.circuitnet.com/catalog/1153804.htm for Solder
Strip, used to remove solder from contaminated gold fingers before
replating.
MikeMcM
-----Original Message-----
From: Dr. Jolyon Browne [mailto:[log in to unmask]]
Sent: Tuesday, December 14, 1999 12:19 PM
To: [log in to unmask]
Subject: [TN] Removing Lead/Tin coating from copper traces
Hi TechNetters:
I would like to remove the lead/tin coating on the external traces of
the PCB in order to expose the copper trace underneath the coating. How
can I do this?
Thanks!
Jolyon
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|