TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Wed, 8 Dec 1999 12:05:36 +1100
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (102 lines)
Well, dear Steve (what's that shooting near by Tulsa ?),
now you start to understand why after two decades of validations and
revalidations and rerererevalidations I still swear by good foam (no clean
flux that is , not Urquell lager).

With NiAu boards i'd have very little chance with spray .
i know 'm in a decadent minority here, but check with those like Wade and
Daan as well,
as far as the quality of fluxing goes (and tidiness) ; spray 's
overengineered underperforming misapplication .
(my opinion , ok, heard/seen/validated all the reasonings ever, don't
shoot!);
my (drastic, sorry) advice 'd be : get the long stone from Wade and switch
back .
Your wave fellow will worship you ; the difference in maintenance and
cleaning is not to be sniffed at .

By the way your QC (nothing personal Nancy [love 'em too])is bit naive
"hoping" dry (nonfluxed)tops will reflow to the tops after re-wave, doesn't
work that way (as you know) .
And hand job is a real desperation , with worst consequences still (as you
know) .

Otherwise you can chat up the QC on reasoning that majority of heavy loaded
P/S cards are SINGLE sided copper,
with no barrel at all ........................etc.

wish yo' luck (sincerely)

cu           paul

-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Tuesday, 7 December 1999 12:21
To: [log in to unmask]
Subject: [TN] Spray Fluxers and Topside solder fillets...


Hi ya'll!

Well, I started wave-soldering with my new beast today, and promptly got
into
a head-butting contest with QA. We switched from foam fluxing to spray
fluxing, and there's problem with QA...(what's new? sheesh...)

The issue that they're having a problem with is the topside fillet
appearance. It does appear that the parts that have a clinch or parts that
have a stand-up/lock-in prep to the leads on them, may not have the
feathered, tapering fillet that rises above the surface of the PCB like we
saw with a foam fluxer, or with leads that drop-in straight to the board. In
my opinion, there's not a problem, and the fillets meet class-II, but here
it's so hard to teach a old dawg new tricks, as far as they're concerned;
"They don't look like they used to...". The fillets are perfectly fine on
the
bottomside, wetting 360-degrees, but on the top they may not fully taper
above the board and may be depressed a bit, but no more than 75%. and the
fillets are wetted to the barrel higher up than it has on the lead...so
under
a microscope, the fillet looks to taper down to the lead. The inspectors are
calling this non-wetting to the lead. I'm saying BS...the fillets are
acceptable. QA is trying to get me to re-wave the boards!...or have the
joints reworked by hand! Sheesh...does it ever end?

Anyways, have those of you that have had experience with spray fluxers ever
run into this issue? I'm using a Kester 2331-ZX (pretty active), but it's a
foam fluxer formula, but I'm still getting good coverage by spraying it. I
was told that I might need to get a spray formula if I didn't get good
coverage.

Any inputs?

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2