In a message dated 12/16/1999 7:46:35 AM US Eastern Standard Time,
[log in to unmask] writes:
> If a water white rosin as received is purified or changed in any way is the
> flux produced from it considered type RE or type RO?
>
RO. No matter how it is purified, it is still a rosin base (RO) rather than
a synthetic resin (RE) base.
Doug Pauls
CSL
##############################################################