Based on Norman Einarson's "Bare Board PWB Design Manual":
FR-4 is a flame resistant glass epoxy.
Tetrafunctional means that there are four sites per molecule after
polymerization, as opposed to two sites per molecule in regular
(difunctional) FR-4. The result is that tetrafunctional FR-4 is denser,
more acid resistant, more stain resistant and has a higher glass transition
temperature. I believe that this will also be more expensive.
Hope this helps.
-Steve
Steven K. Lustig
Process Engineer
EMS Technologies, Inc.
Norcross, GA
(770) 263-9200 x4714
[log in to unmask]
-----Original Message-----
From: Parvez M.S. Patel [mailto:[log in to unmask]]
Sent: Tuesday, December 07, 1999 9:43 AM
To: [log in to unmask]
Subject: [TN] What do we mean by FR-4
Hi everybody,
I was wondering what does FR-4 stand for..
and what do we mean by tetarfunctional Fr 4 (as in boards)
Thanks in advance
Parvez M.S. Patel
Graduate Research Associate,
Universal Instruments Corporation,
SUNY - Binghamton, New York.
Ph: 607 779 7215(O)
Fax: 607 779 4646
*************Equilibrium is death. Seek persistent
non-equilibrium***************
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|