Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Tue, 7 Dec 1999 18:33:25 +0800 |
Content-Type: | multipart/mixed |
Parts/Attachments: |
|
|
Hi Edward
Did your company using the 106A type or the improvised 106A ( X
) type . We had change to the one with the PC 106 one
recently and it seem that the entek thickness is more difficult
to control than the older version .
According to Ethone , the main advantages of this newer version is
to prevent " gold tarnish " on top of gold surface . Would like
to heard your side experience
W L lee
WUS Printed circuit Singapore
edward edward szpruch <[log in to unmask]> on 12/07/99 06:03:16 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to edward edward szpruch <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Wei Leong Lee/WUSSG)
Subject: Re: [TN] Difference between OSP & Entek '106A'
Entek 106+ is one of the OSP`s on the market.
regards
Edward Szpruch
Eltek , Manager of Process Engineering
P.O.Box 159 ; 49101 Petah Tikva Israel
Tel ++972 3 9395050 , Fax ++972 3 9309581
e-mail [log in to unmask]
> -----Original Message-----
> From: Ko Adeline-FSGA2298 [SMTP:[log in to unmask]]
> Sent:
ג דצמבר 07 1999 11:36
> To: [log in to unmask]
> Subject: [TN] Difference between OSP & Entek '106A'
>
> Hi to all,
>
> I was totally confuse by the OSP & Entek 106A finishing.
> What is the difference between OSP & Entek 106A?
> In term of :-
>
> 1) Cost
> 2) Electrical performance
> 3) Process issue
> 4) Stencil thickness
>
> Thanks!
> Adeline Ko
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|