How long for? Don't know of a metallic treatment as such, but there are some filled resins
and elastomers you could use as a surface treatment. These are either extremely hard
ceramic filled products or softer rubber or filled epoxies. These later are designed to
trap impinging particles on the surface which then then wear out further impinging
particles rather than the underlying metal.
Come back direct if you need more details.
Mike
----- Original Message -----
From: Vaughan, Ralph H <[log in to unmask]>
To: <[log in to unmask]>
Sent: 02 December 1999 18:50
Subject: [TN] anti-abrasion finish
> Hi TN,
>
> A follow-up query to a recent posting about sand-type abrasion for you
> metalheads (Dave H., you there?); Is there a metal finish that will
> withstand rubbing wear from aluminum oxide powder? we have tried tungstun
> carbide and stellite with 'no joy'. Any light bulbs going on?
>
> Thanks for thinking>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|