Regarding the RH in a PCB assembly facility, besides ESD, the RH (as well as
ambient temperture) affects the behavior of the solder paste in process.
Both No-cleans and water solubles are hydroscopic in that they absorb
moisture from the air. Hence, too high RH will result in a change in solder
paste printing characteristics and/or results ranging from shorter work life
to dewetting and, yes, the ever-annoying solder balls.
Too low a relative humidity will adversely affect OA solder pastes in that
they are effectively being dried out. Again, symptoms I've observed include
shorter work life, shorter tack times, dewetting, non-wetting and solder
balls.
Most solder pastes seem to desire a range of between 35 - 75% RH. When I do
a Process Audit for a client, I specifically look for a means of reading and
recording RH on an ongoing basis. Those chart recordings can be useful in
defect analysis.
Another reason to keep RH within a decent level is for the comfort of your
workers. Just a thought!
Regards,
Phil Zarrow
Process Consultant
ITM, Inc.
Durham, NH USA
www.ITM-SMT.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|