Craig, Yes HCl is a step between Ni and Au plate. It is used to
activate the Nickel surface to accept gold plating for better
adhesion.
Mike Doty
PE Hadco TCE
______________________________ Reply Separator _________________________________
Subject: [TN] HCl clean of Ni/Au plating
Author: Craig Hillman <[log in to unmask]> at smtplink-hadco
Date: 12/21/99 5:00 AM
Hello Technetters,
Is HCl clean of the nickel pads sometimes a step in the Ni/Au
plating process? If it is, why is it done?
Thanks for your response,
Happy Holidays,
Craig
Dr. Craig Hillman
CALCE Electronic Products and Systems Consortium
University of Maryland
College Park, MD 20742
(301)-405-5316
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|