TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 21 Dec 1999 13:51:59 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
Larry Tawyea <[log in to unmask]>
Parts/Attachments:
text/plain (33 lines)
In a message dated 12/21/99 11:20:32 AM Central Standard Time,
[log in to unmask] writes:

<< Hello Technetters,

         Is HCl clean of the nickel pads sometimes a step in the Ni/Au
 plating process? If it is, why is it done?
  >>

Craig,

When you say plating the nickel pads I'm going to assume you are doing a
selective plate as opposed to a pattern plate,  In this case there are
process steps between the nickel and gold plate.  The purpose of the HCl
clean is to remove the nickel oxide that forms very quickly when the nickel
is exposed to air.  Hope this answers your question.

Larry Tawyea

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2