Ivan,
You may get a bunch of opinions on this one.
I highly suggest that you contact your London Chemical (Lonco) Technical
Representative as soon as possible. It's his (or her) responsibility to
provide you with all the information relating to their product.
Peter A. Phillips
Honeywell Inc.
Defense Avionics Systems
9201 San Mateo Blvd. NE
Albuquerque, NM 87113-2227
[log in to unmask]
505.828.5078…work
505.530.7147…pager
505.828.6709 ... fax.
M/S NM75-D09A
> This message is intended for the individual or entity to which it is
addressed, above. If you are not the intended recipient, please do not
read, copy, use or disclose this communication to others. Please notify the
sender by replying to this message, then delete it from your system.
> Thank you.
>
-----Original Message-----
From: Ivan Barrios [mailto:[log in to unmask]]
Sent: Thursday, December 16, 1999 1:48 PM
To: [log in to unmask]
Subject: [TN] Flux storage
Recently, the flux we are currently using (Lonco Organo-Flux 3355 Highly
active
halide containing water soluble flux) had very low readings on density.
(0.845
@ 13C). It was stored in an outside chemical room, roof covered but the
door is
chai link fence and about 10 ft wide. The temperature got down to +20 F
overnight, and I am wondering if it would be possible to have the flux and
the
thinner separate at this low temperature, with the thinner floating to the
top
of the container and the flux depositing in the bottom of the barrel.
Are there any special guidelines I should follow for storage of the flux?
(Any
type, not just this specific one)
As continued to use this flux, the readings have gone back to normal, and
never
saw any soldering issues related to flux problems. Any and all answers
appreciated.
Ivan Barrios
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|