Paul,
I suspect the use of Palladium is to prevent "black pad" since it has
been found to occur during the immersion gold process. With a Palladium
layer on the nickel, hyper corrosion of the nickel should not occur (in
theory). (it still sounds expensive).
Thanks
Ryan Grant
Process Development Engineer
MCMS
(208) 898-1145
FAX (208) 898-2789
[log in to unmask]
No problems 1-5 Darrel, just ask him why standard (flash) NiAu would not
be
sufficient .
From distance i can't see the need for Pd instep expense.
Check net's archives , all there
pk
-----Original Message-----
From: Darrel Therriault [mailto:[log in to unmask]]
Sent: Tuesday, 7 December 1999 4:59
To: [log in to unmask]
Subject: [TN] Ni/Pd/Au
TechNet,
A PWB supplier is recommending a Ni/Pd/Au finish for .062" and .093"
FR-4
PWB
with mixed PTH/SMT components, as well as press fit connectors.
Any comments/guidance, pro or con, regarding :
1. Intermetalics
2. Rework cycles
3. Gold embriddlement
4. Fine pitch or BGA components
5. Pressfit
All info appreciated.
Regards.......DT
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|