Hi Kim!
The hollow fiber means the glass fiber which has a capillary in itself.
If the molten glass contains a sufficient level of impurities or gas bubbles,
air will become trappeed inside a fiber.
See the following material:
Anand A. Shukla,etal."Hollow Fibers in Woven Laminates" Printed Circuit Faburication,
Vol.20,No.1,p30-32(1997.1)
Regards,
Motoyo Wajima
Enterprise Server Division,Hitachi,Ltd.(Japan)
=?euc-kr?B?sei03r+1IML3wOUgwPzA2iDB9cbysPjA5cewwfq6uMH1xsA=?= $B$5$s$O=q$-$^$7$? (B:
> Dear Technetters:
>
> Have you ever experienced or heard of hollow fiber ?
> Is this in the state of hollowing between fibers or fiber itself?
> For the former, I think poor soaking of resin is the cause and the latter
>is intentionally developed
> fiber to reduce Dk.
> Do you have any idea to improve soaking tight bundle of fiber?
> Any comment to this is appreciated.
>
>Tal Young Kim
>Manager, Quality Assurance Team
>Doosan Corporation Electro-Materials BG
>Tel : 82-445-820-8451
>Fax : 82-445-820-8300
>E-mail:[log in to unmask]
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
***********************************************
Motoyo Wajima
Enterprise Server Division,Hitachi,Ltd.
1 Horiyamashita
Hadano-shi,Kanagawa-ken,259-13 Japan
E-mail:[log in to unmask]
Fax:+81-463-88-2935
***********************************************
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|