Steve,
We have the same problem when we use the Komoto Pake pens. We do not use them for much
anymore. What I do is buy small batches of liquid resist. We touch up the dry film
with that then cure under a small black light that you get at the hardware store or
McMaster Carr catalog.
If you have any questions call or send me a note
Chuck Brummer
818.734.4930
[log in to unmask]
[log in to unmask] wrote:
> To All,
> I was wondering if there is such a thing as a fully aqueous touch-up
> pen. I am having trouble with one of my resist strippers removing the
> touch-up pen ink. It is the Kimoko (I think that's the name anyway) touch-up
> pen. Maybe someone has a suggestion for another touch-up pen with ink more
> easily removed by resist strippers.
>
> Thanks,
> Steve Wentz
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|