TECHNET Archives

November 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Mcmaster, Michael" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 24 Nov 1999 08:41:20 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (114 lines)
Phil

Thanks for the proofread.  I need to get that fixed.


        Mike McMaster
        RF Product Engineer
        Merix Corporation
        503-992-4263


        ----------
        From:  Phil Crepeau [SMTP:[log in to unmask]]
        Sent:  Monday, November 22, 1999 5:21 PM
        To:  [log in to unmask]
        Subject:  Re: [TN] Looking for list of prepreg and core thickness
for FR-4

        hi,

        i think you need to do a sanity check on the data at this site.  for
        example, they state that the thickness of 1/4 oz/ft2 copper is 3
mils.  this
        is a typo.  the thickness of course is about 0.3 mils.  the
guideline on a
        lot of data you get on the internet is 'caveat emptor'.  i heard
once heard
        it said that there is a lot of information on the internet, but
knowledge is
        not guaranteed.

        phil crepeau

        -----Original Message-----
        From: Stephen R. Gregory [mailto:[log in to unmask]]
        Sent: Monday, November 22, 1999 4:44 PM
        To: [log in to unmask]
        Subject: Re: [TN] Looking for list of prepreg and core thickness for
        FR-4


        In a message dated 11/22/99 3:54:13 PM Central Standard Time,
        [log in to unmask] writes:

        > I am looking for a list of standard thicknesses for FR-4 prepreg
and cores
        >
        >  Can anyone help?
        >  Barbara Burcham @ Fairfield
        >  Houston

        Hi Barbara!

        Merix has a pretty decent page about FR-4 prepreg properties at:

        http://www.merix.com/main_res.html

        Click on DFM in the column at the left of the page when it opens...

        Hope this helps...

        -Steve Gregory-

        ##############################################################
        TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        ##############################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following
        text in
        the body:
        To subscribe:   SUBSCRIBE TECHNET <your full name>
        To unsubscribe:   SIGNOFF TECHNET
        ##############################################################
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information.
        If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
        847-509-9700 ext.5365
        ##############################################################

        ##############################################################
        TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        ##############################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
        the body:
        To subscribe:   SUBSCRIBE TECHNET <your full name>
        To unsubscribe:   SIGNOFF TECHNET
        ##############################################################
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information.
        If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
        847-509-9700 ext.5365
        ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2