     Oh, yeh. One more reference: James Blankenhorn, thru SMTPLus, inc.,
     has put together a pretty good package for this, which comes with a
     book and decent software. His calculations are for (at least my
     experimentation shows this) 100% fillets and LOTSA solder. Good info
     there, especially for someone new, book/software is titled,
     surprisingly enough, "Using Solder paste for Leaded Parts on SMT
     Assemblies". Hey James, where's my commission?? ;')
     regards, Jeff.


______________________________ Forward Header __________________________________
Subject: Re: [TN] Intrusive Reflow
Author:  Jeff Hempton <[log in to unmask]> at Internet
Date:    11/16/1999 11:23 AM


     Steve, I was out for a few days on travel, but wanted to share more
     info with the group on this. Also, I have used the AMP calculations
     successfully that was referenced on the Technet, for some of the first
     PIH projects. One thing I did not see referenced was the fillet
     requirement. Many times your criteria can live with less then 100%
     fillet....Phil Zarrow (hello Phil, ya out there?) had some interesting
     formulas that had a FACTOR in his equations based on the amount of
     fillet required.  He was pretty open to sharing this in the past, his
     e-mail is [log in to unmask], or phone at 603-868-1754. Also, an
     interesting alternative to PIH is solder-loaded headers, see this on
     TEKA's website at w3.bbsnet.com/TEKA (that's an old address, they may
     have a new one). Anyway, hope this info helps. Feel free to contact me
     anytime if more questions, PIH is a pet project of mine. Regards.
     Jeff Hempton
     United Technologies Electronic Controls


______________________________ Forward Header __________________________________
Subject: Re: [TN] Intrusive Reflow
Author:  "Stephen R. Gregory" <[log in to unmask]> at Internet
Date:    11/11/1999 4:21 PM


In a message dated 11/11/1999 2:28:36 PM Central Standard Time,
[log in to unmask] writes:

<< Hey, Steve!
    I've got an article in front of me that I pulled from AMP's web site
 some time ago.  It has lots of information that AMP developed for intrusive
 reflow.  The URL shown on the top of the sheet is
 http://WWW.AMP.COM/product/articles/dd66.html.  There are follow-on pages at
 /dd66a.html, etc.
    The only problem is, I can't seem to go back there by typing the
 URL, and I can't find any such article on the AMP site by going to
 product/articles. >>

Hi Greg!

You're not the only one who has directed me towards that article. It was
referenced in some archived TechNet posts I read too...it had to be there
somewheres since I seen so many references to it. I too had trouble finding
that article. But being the "sleuthy" guy I am, I found it!

Go to the main page http://www.amp.com, then click on the "products" tab at
the top of the opening page. When the next page opens towards the top
right-hand side of the page there will be a link called "Technology Journal",
click that and the next page that opens there will be a links column on the
left hand side of the page. Down towards the bottom there's an "other" link
just under "Technology", click "other" and viola, there's the article!
"Solder Volumes for Through-Hole Reflow Compatible Connectors"

Amp musta' re-arraigned things at their site, that's why it was so tough to
find...

Thanks!

-Steve Gregory-

P.S. Thanks too Scott, John, and Justin, for the articles you sent me as
well!

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2