Yes you are right. One of the problems that will arise when using lead free
solder is the cracking of ceramic chip components. However, also lead free
solder creeps. This means, the stress occurring in the component does not
only depend on the temperature range but also on the temperature ramp.
However, I don't have any data.
Best regards
Guenter
Guenter Grossmann
Swiss Federal Institute for Materials Research and Testing
8600 Duebendorf
Switzerland
##############################################################