I have heard of ceramic caps cracking if the pads they are mounted to are wider
than the body of the cap. It has been suggested to make the pads slightly
narrower than the body of the part.
Charlie B.
Wanner Bernhard <[log in to unmask]> on 11/10/99 10:57:00 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
Wanner Bernhard <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Charles Barker/US/I-O INC)
Subject: [TN] 1812 capacitors on FR-4
-----Urspr?ngliche Nachricht-----
Von: Matthew Lamkin
[SMTP:[log in to unmask]]
Gesendet am: Freitag, 25. Juni 1999 09:26
An: [log in to unmask]
Betreff: Re: [TN] FW: What it would be like living in
Australia
Well I don't know about being a joke, but I've saved it as a handy
little utility.
By selecting it from my start menu I can now turn a PCB that I am
working on upside down to view it from another angle.
Something that I have occasionally wanted to do. I can remember
actually
going as far as turning the monitor on its side
before, just so that I could view something from a different angle
without upsetting everything else in the PCB file.... <g>
Hi technos, we have some problems with 1812 (and also with 1210) capacitors
on FR4 because cracks at the corner. Is there any size limit for SMT cap's
on FR4 (may be different classed for different application temperatures)?
Thanks, Bernhard, Z?rich
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|