In a message dated 11/11/1999 11:47:23 AM Central Standard Time,
[log in to unmask] writes:
<< I have an application where I need to mask off a through-hole SIP
through wave solder. Washable liquid mask is getting on closely adjacent
bottom-side SMT components, and I can't justify an automated dispenser with
current volumes. I remember a company back in the days of when through-hole
was king (waaaay back there) that made high-temp filled plastic masking
thingamajigs that fit standard DIP/SIP patterns. You just dropped them in
the hole pattern before wave, then removed and reused them after wave.
Anybody out there know what I'm talking about, and who makes them?
Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX 77478
(281) 243-5639 Phone
(281) 243-5539 Fax
[log in to unmask] >>
Hi Mike!
You call those things; "Thingamajigs" huh? I always called them
"Whatchamacallits"
Did a search on "whatchamacallits" and came up with this:
http://www.whatchamacallit.com/
Don't think I'll be getting in touch with Sam or Dan though...hehehe
Seriously, here's three places that make hi-temp tapered plugs in all kinds
of sizes that's
used for powder coating and plating. Might give them a call and see if they
have something
off the shelf. All the plugs I seen on their pages are individual plugs
though. But you could
have these places die-cut .100" spaced holes in some strips of the same
material that the
plugs are made of, buy the individual tapered plugs, then insert and glue the
plugs into the
strips. Might be a little work at first, but then ya' got what you're looking
for!
http://www.hi-techflex.com/
http://www.harmancorp.com/
http://www.sandy.com/echohome.html
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|