Ingemar: Indium is used for gaskets and similar becuase it is very soft and deforms
easily, retains softness over a wide range of temps (down to cyrogenic). Tin would
probably be too hard, but some people do use tin/indium alloys to cut costs a bit. also
being slightly harder makes big washers / floppy shapes easier to handle. You can also use
silver based elastomers from specialist suppliers.
ps How's the bubbling.
Mike Fenner
Bonding Services & Products
T: +44 1295 722992
F: +44 1295 720937
For product info visit www.belzona.com
----- Original Message -----
From: Ingemar Hernefjord (EMW) <[log in to unmask]>
To: <[log in to unmask]>
Sent: 19 November 1999 07:24
Subject: [TN] Ku-band waveguide gasket
> Hi, an unusual question, but I see many radar guys are reading also in TechNet. So, what
sealing gaskets do you use for flange-to-flange sealing, electrically as well as gas
tightening? We tried Indium, works well, but the price is immense. If the waveguide is
ordinary Al with Nickel+Chromate, then what about Tin gaskets? Atmosphere around is dry
and you have that Nickel barrier. Copper seems to be too hard. Any good idea?
> Ingemar Hernefjord
> Ericsson Microwave Systems
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|