Does anyone have the telephone number for Contamination Studies Laboratories
or that of Doug Pauls. And, can anyone tell me in paragraph D-4.3.5.1 of
IPC-J-STD-001a, what the control samples are and what the
sentence,"Additionally,six control boards(three for cleanliness testing and
three for SIR testing) shall not be processed beyond the initial pretest
preparation" means. What paragraph describes pretest preparation?
What is the pretest preparation process?
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|