I do not recommend HAL for UHF boards: the flux residues are damn hard
to remove and the hygroscopicity of them may be limitative, especially
if you do decide on an FR-4. You may also care to consider 35 µm copper
(1 oz) on the inner layers for a better connection to through
holes/vias. Does the fact that 2 x 1080 is specified suggest controlled
impedance? If so, be prepared to find the high resin:glass ratio will
give a slightly higher dielectric constant than a more usual build. Also
HAL is definitely NOT recommended for controlled Zo.
Brian
Ko Adeline-FSGA2298 wrote:
>
> > Hi there,
> >
> > My engineer is asking me to design a 900Mhz 4-layer brd using the
> > following information.
> > As this is my first time doing such a high freq brd.
> > I wish to know, is this PCB material perform excellent in high freq.
> >
> > PCB Info
> > Top layer --> 1/2 oz copper
> > Prepreg --> 2 X 1080
> > Layer 2 --> 1/2 oz copper
> > Prepreg --> 2 X 7118
> > Layer 3 --> 1/2 oz copper
> > Prepreg --> 2 X 1080
> > Bottom --> 1/2 oz copper
> >
> > Brd finishing thickness : 0.031" +/- 0.005"
> > Material : FR4.
> > Plating : Tin / Lead 63/37 HAL
> >
> > Thanks & Best Rdgs
> > Adeline Ko
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|