We are located in the mid-west, Indiana to be exact. Our factory is very well
controlled, humidity and temp wise. No solder splash or balls seen. Just the
occasional void. Thanx Joyce for your input!
______________________________ Forward Header __________________________________
Subject: Re: [TN] ASSY: SMD solder voids
Author: joyce <[log in to unmask]> at Internet
Date: 11/11/1999 6:23 PM
aged solder paste sometimes have void problems...usually, under high RH% MFG
condition...If you are "lucky", you would see solder splash coupled with
voids (solder balls, etc), otherwise, it is not so easy to spot the problem
...(it was a hard lesson to learn many years ago).
where are you located? warm and high RH?
jk
At 10:45 AM 11/11/99 -0500, you wrote:
> Hi gang,
> We are cross-sectiong some solder joints, and are seeing some
> voiding inside the joint itself, that appears to be "air pockets" that
> were inside the joint when reflowed. There is no visible indication
> externally of any voiding, but it is fairly prevalent inside various
> component solder joints when cross-sectioned.
>
> I cannot find criteria or mention of this in the specifications I
> have. ANSI/IPC-A-610A shows voiding criteria for thru-hole components,
> but none for SMD.
>
> Does anyone have knowledge they can share on this topic? Is there a
> spec on internal SMD joint voiding available? Do you guys and gals see
> this occasionally in your joints?
>
> Please, enlighten me with your collective wisdoms!
> TIA!
>
> Jeff Hempton
> United Technologies Electronic Controls
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|