TECHNET Archives

November 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"McMonagle, Michael R." <[log in to unmask]>
Date:
Fri, 12 Nov 1999 08:52:25 -0600
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "McMonagle, Michael R." <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
Steve,
        If you can get away with it without hosing up your fine pitch print,
a dual print cycle will also give you more paste into the holes.

Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX  77478
(281) 243-5639 Phone
(281) 243-5539 Fax
[log in to unmask]

> -----Original Message-----
> From: Stephen R. Gregory [SMTP:[log in to unmask]]
> Sent: Friday, November 12, 1999 7:41 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] Intrusive Reflow
>
> In a message dated 11/12/1999 3:54:06 AM Central Standard Time,
> [log in to unmask] writes:
>
> << A properly filled 40 mil hole contains more paste than a 70 mil stencil
> aperture, so please don't forget to pay attention on how to get the paste
> INTO the holes  Experiment with things like squegee speed, pressure, and
> solderpaste rheology.
>
>  Daan Terstegge >>
>
> Thanks Daan! I'll be running my squeegee speeds real slow to allow as much
> paste to roll into the holes as possible, and I'm using metal
> blades...appreciate the input!
>
> -Steve Gregory-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2