Hi Steve
We're both slightly nervous. I got my first intrusive reflow stencil in
today. Can't wait to try it. Like your experience the uncontrolled tests
were very encouraging. Try www.itm-smt.com and go to articles. I can't
really comment on your choice of aperture size without knowing the lead area
filling the hole and thus the solder volume required. The referenced
article has a suggested formula. Also try the Bob Willis web site. Good
luck
John Thorup
> -----Original Message-----
> From: Stephen R. Gregory [SMTP:[log in to unmask]]
> Sent: Thursday, November 11, 1999 11:52 AM
> To: [log in to unmask]
> Subject: [TN] Intrusive Reflow
>
> Hi ya'll!
>
> I'm getting ready to do some intrusive reflow on this board we got
> here...(this is my first time! I'm s-o-o-o nervous...not really...well,
> maybe
> a little...hehehe) Anyways,
> the parts are going to be 2, 20-pin SIP sockets. The board is .063" thick,
> the holes
> are spaced .100" apart, and the hole diameter is .040". I'm trying to
> decide
> how big I should make my apertures.
>
> I've looked at all the archive postings (there are a 168 of them on
> intrusive
> reflow) to see if anybody posted any recommended stencil thicknesses,
> and/or
> aperture sizes,
> but there was none. I looked on the web, but couldn't find any real
> guidelines either...
> (hmmmm, something I couldn't find...now THAT's a change!)
>
> I need to keep my stencil thickness at 6-mils, 'cause I've got some 20-mil
> pitch stuff on the same side. I was thinking of doing .060-.070" diameter
> circles over the holes...
> does that sound okie-dokie?
>
> I did a little test with the SIP socket and a syringe full of solder
> paste. I
> drew a bead of paste (about .030" dia.) down the row of holes and dropped
> the
> connector in, then reflowed it. Then I got my dremel tool out and did me a
> rough cross section to check the barrel fill. It actually wasn't too
> bad...there were about 2-3 holes that were a little shy volume-wise but
> that
> was because (I think) the solder wicked over to the holes next to it
> because
> of the continuous bead of paste I had laid down. That shoudn't happen when
> I
> have individual deposits of paste for each hole.
>
> So how big should I make my openings? Did I guess right at .060-.070"?
>
> -Steve Gregory-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|