Wanner,
Case size 1825 and larger should not be used on FR4 due to the CTE missmatch
on a ceramic part that large, however the 1812's should be OK. I would not
look to the FR4 as
the problem but look at the Cap vendor and whether the caps have been on the
shelf too long'and moisture has
invaded them. They may need to be pre-backed if the later problem is it.
Again verify with your cap vendor also.
Bob Wolfe
Executone
Wanner Berndard wrote
Von: Matthew Lamkin
[SMTP:[log in to unmask]]
Gesendet am: Freitag, 25. Juni 1999 09:26
An: [log in to unmask]
Betreff: Re: [TN] FW: What it would be like living in
Australia
Well I don't know about being a joke, but I've saved it as a handy
little utility.
By selecting it from my start menu I can now turn a PCB that I am
working on upside down to view it from another angle.
Something that I have occasionally wanted to do. I can remember
actually
going as far as turning the monitor on its side
before, just so that I could view something from a different angle
without upsetting everything else in the PCB file.... <g>
Hi technos, we have some problems with 1812 (and also with 1210) capacitors
on FR4 because cracks at the corner. Is there any size limit for SMT cap's
on FR4 (may be different classed for different application temperatures)?
Thanks, Bernhard, Zürich
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|