For years we have used type R flux when working with stranded wires. Not
only does the solder wick up under the insulation (into the wire core) so
does the flux. Since type R does not contain activators there is little to
no chance for corrosion. The second key is to reduce the volume of flux
usage to only that which is volitized in the soldering process (ie. use only
minute quantities of flux always, excess is also waistful).
Ron Dieselberg
-----Original Message-----
From: Miguel Vallejo [mailto:[log in to unmask]]
Sent: Saturday, November 06, 1999 02:57
To: [log in to unmask]
Subject: [TN] Soldering Stranded Wires
Hi,
Is there a documented reference for recommended flux type for soldering
stranded wires?
Currently, we only use RMA or No-clean types. My understanding regarding
water soluble fluxes is that they are highly corrosive and that it's
difficult (if not impossible through a regular cleaning process) to
remove the flux from underneath the insulation. I'm trying to
substantiate this claim. Any help will be appreciated.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|