Stephen,
For gold plating with nickel underplate, as used in connector applications,
it used to be MIL-G-45208 (cancelled 4/7/98). It has been replaced by ASTM
B488.
Hope this is what you are seeking.
R. G. Blomberg
Honeywell –SASSO
Staff Production Engineer
(727) 539-5534 voice
727-539-4469 Fax
[log in to unmask]
-----Original Message-----
From: Stephen Ayotte [mailto:[log in to unmask]]
Sent: Tuesday, November 09, 1999 5:50 AM
To: [log in to unmask]
Subject: [TN] Mil Spec for nickel and gold thickness
What is the mils spec number for nickel and gold thickness? thx
Stephen Ayotte, IMD Product Quality Engineer
Essex Junction, Vermont
Dept. N62V, Bldg. 966
Phone (802) 769-4775, t/l 446-4775
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|