Ivan,
You could put a plastic spacer under LED and remove it after wave solder.
Ivan Barrios wrote:
> I am currently having an issue with blowholes on TH components. What I have
> concluded is that the components are too tight and sit flush against the top of
> the board. When they go through wave solder, the outgassing has no way to go but
> down towards the wave solder. We have tried loosening up components but then we
> incurr having the LED's uneven after wave solder (and the LED's do not match up
> to the corresponding window in the enclosure) and are currently looking for an
> alternate LED that has standoffs so that the plated barrel is not sealed at the
> top. My question is: Is there anything that can be done process wise to reduce
> this defect? Thanks to all for your input
>
> Ivan Barrios
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
--
____________________________________
Regards,
Pratap Singh
Tel./Fax: 512-255-6820,
e-mail: [log in to unmask] or [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|