TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 11 Oct 1999 20:13:24 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (42 lines)
In a message dated 10/11/99 6:58:33 PM Central Daylight Time, [log in to unmask]
writes:

> Looking for testing laboratory in San Jose bay area for fab cross-section.
>  Are there any IPC approved?
>
>  re,
>  ken patel
>  ______________________________________________________
>  Ken Patel                       Phone:  (408) 490-6804
>  1708 McCarthy Blvd.             Fax:    (408) 490-6859
>  Milpitas, CA 95035              Beeper: (888) 769-1808

Ken,

This place ain't in the Bay Area, but from recent experience, they don't need
to be.

Go to: http://www.tracelabs.com/

You fed-ex overnight what you want microsectioned, they get it, and within
about 4-6 hours they have the results complete with digital images that they
will send to you, and a basic analysis report of the problem. They can get
more in-depth if you want (for a little more). They charge $54.00 a
microsection. Recommend them highly.

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2