Cute. Hope your (much) better half drops hairdryer into your bath tub (aka
craftcarrier) one day .
You have earth leak tripper home ? paul
-----Original Message-----
From: Ingemar Hernefjord (EMW)
[mailto:[log in to unmask]]
Sent: Monday, 11 October 1999 17:34
To: 'TechNet E-Mail Forum.'; 'Paul Klasek'
Subject: RE: [TN] Conductive Floors ...
So the word "conductive" is the same as "grounded". How then can the steel
deck of craftcarrier be grounded? There is only water around./Ingemar
"CONDUCTIVE" is used only in ammunition and fireworks factories, explosive
compounds generally ;
otherwise with powered equipment on the floor it can kill .
Dissipative vinyl would be best way to go ;
The self dissipating(with some humidity in the air) paint on concrete does
not last in traffic spots more than couple of months .
Bare concrete is neutral, but dusty; sealed with epoxy is static generating
, not dissipating .
Doug, the archives are full of ESDAssociation references ;
which I'd find more practical than BS or DIN,
you can get them on disk as well .
Repeating myself again : make sure you have 1Mohm resistor somewhere between
ground and grounded .
There is a legal difference between conductive and dissipative surface when
it comes to accidents ;
and even ESDA standards underline the safety as a logical PRIORITY:
for example whereas SSteel cabinet covers are normally grounded direct ;
in instances of working with power equipment for example on SSteel bench ;
that bench should be grounded indirect (with resistor in the path) .
ESD's grounding does have similar character as CO2 versus CO ;
TOO simple and common perceptions can be deadly in certain circumstances
without lateral thought .
Similar to those having gas heaters not flued outside .
Get the standards Doug, they're absolutely essential;
this is one of few fields where "common sense" is not desirable .
Paul Klasek
ResMed
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|