TechNet,
We have sporadic problems with the copper level rising in our solder pot. We
reduce the temp and dross each morning. Could you recommend a specific PM
program to keep our SnPb clean? We believe per the certicates of analyses
that
our supplier gives us good product. Any other reasons it might rise?
Thanks,
Green
##############################################################