TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Vaughan, Ralph H" <[log in to unmask]>
Date:
Thu, 28 Oct 1999 13:15:02 -0600
Reply-To:
Subject:
From:
Joe Wojniak <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (64 lines)
Related to sand and aluminum oxide:

I was watching a TV show doing a documentary on etching pictures into glass
by sand blasting.  The artist was using aluminum oxide instead of sand
because there are apparently health risks associated with sand.

Don't know if it's true or just Hollywood...

-Joe Wojniak

 -----Original Message-----
From:   TechNet [mailto:[log in to unmask]]  On Behalf Of Vaughan, Ralph H
Sent:   Thursday, October 28, 1999 9:33 AM
To:     [log in to unmask]
Subject:        [TN] sand-man

For anyone who would like a diversion from the assembly processes, I have a
different question.

My Army customer is simulating field testing of a weapon system to check the
abrasion resistance of some treated metal surfaces (tungsten carbide) that
rub together during flight.  The 'sand' that they are using to contaminate
these areas is aluminum oxide.  Needless to say, excessive scoring is
observed on the metal faces.  My contention is that sand is primarily
quartz, or silicon dioxide, which is softer than the Al2O3, and the system
is being over-tested.

Anyone have a notion of the acceptable sand type used in environmental
tests?

Thanks

Ralph Vaughan
Boeing-Fleming

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2